A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Spinner for SOG
Re: Spinner for SOG
1998-08-20
[email protected]
1998-08-19
Shekhar Bhansali
1998-08-19
Ash Parameswaran
Re: Spinner for SOG
Ash Parameswaran
1998-08-19
The SOG manufactureer usually give the
thickness versus spin speed data.


Any lithographic spinner should do the job.

We have done 3 to 4 microns thick, however using
multiple coats.

Ash Parameswaran