MEMSnet Home: MEMS-Talk: Gold Etchant with selectivity over Mo (Kevin Paul Nichols)
Gold Etchant with selectivity over Mo (Kevin Paul Nichols)
2008-07-25
Harry van der Zanden
Gold Etchant with selectivity over Mo (Kevin Paul Nichols)
Harry van der Zanden
2008-07-25
I would try a proprietary alkaline gold stripping solution like it is sold
by companies as Technic / Rohm and Haas / MECO or Enthone (I'm not trying to
make this a commercial) but these goldstripping solutions barely attack
nickel, so I expect nearly no attack on the Mo as well. However I never
tried it out.

Good luck,

Harry
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.