Polyimide
2008-08-22
dai truong
2008-08-24
Tolga YELBOGA
2008-08-25
dai truong
Polyimide
dai truong
2008-08-22
Hi all,
I have used polyimide SU8-2000.5 with a process as following:

·         Spin PR (SU8 2000.5): 10 seconds
500rpm and 30 seconds 3000 rpm (expected PR film thickness 500nm)
·         Soft bake: 60 seconds
·         Expose: 5 seconds
·         Post Expose bake (PEB): bake at 950C
in 90 seconds
·         Development: 70 seconds and rinse in
IPA 10 seconds
 .       Hard bake (Cure): 2000C
in 15 mins

but after all, the SU 8-2000.5 film thickness is only  about 300nm, and on the
surface some holes occur.  how I can get 500nm-thickness film and cure
temperature is enough.
thanks


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review