Effect of high temperature on gold.
2008-09-19
abhaya joshi
2008-09-19
Michael D Martin
2008-09-19
Roger Shile
2008-09-19
Sood, Sumant
Effect of high temperature on gold.
abhaya joshi
2008-09-19
Hi all

i am having gold layer of 1.5 um on Si3N4 coated Si wafer.
i would like to treat this wafer at 650C.
what will be the effect on gold.

in my previous experiment, the when i coated the gold on silicon and treated
for 600C., i observed the re-flow of gold.
can any one tell me the cause for this?

-abhay joshi
Research scholar,
university of pune.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics