Dear members,

We received Fox12 resist (negative resist HSQ for e-beam) a week ago. We
stored it at 8°C.  We let the bottle in ambient air only during a few
hours when we spincoat the resist. Today, the phase of the resist seems
to have changed, looking like jam. We don't understand what happens, is
it due to the repeated variation of temperature? How do you preconise to
store the resist?

Thank a lot

Paolo Bondavalli
Nanocarb Lab.
Equipe mixte Ecole Polytechnique/Thales
THALES RESEARCH AND TECHNOLOGY
Route Departementale 128
F91767 Palaiseau Cedex
(FRANCE)
Tel : 01 69 41 58 83
Fax : 01 69 41 57 38
Email : [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering