RIE etch of photoresist
c c
2008-12-09
Hi,

I Want to etch photoresist wall, with angle near 90°, size near 20µm:

Is it possible to do that with a Plasma with O2-CF4-N2 800W?

What flows can i use for O2-CF4-N2?

Thanks.