Re: PMMA on SiO2
1998-09-22
Yohannes
1998-10-02
Armin Kuebelbeck
Re: PMMA on SiO2
Armin Kuebelbeck
1998-10-02
Try to use HMDS vapour as an adhesion promotor. Union Carbide has
although some Silane called adhesion promotors. They are in principle
Trimethylethocxy (or methoxy) derivates with a chain group which has a
functional groug. This group can be e.g. an epoxy (for adhesion
promotion in epoxies or an acryl group for you case.

Best regards

Armin

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review