MEMSnet Home: MEMS-Talk: Au electroplating on Al substrate
Au electroplating on Al substrate
2009-01-07
Denis Petrov
2009-01-07
Alexandre BOE
2009-01-07
Oakes Garrett
2009-01-08
Ravi Shankar
2009-01-08
IGOR KADIJA
2009-01-08
Heather Broadbent
2009-01-08
Edward Sebesta
2009-01-08
Wilson, Thomas
2009-01-08
Brad Cantos
2009-01-08
Huihang Dong
Au electroplating on Al substrate
Wilson, Thomas
2009-01-08
Regarding the aluminum oxide formation and the use of Au as a seed layer .... I
wonder if Au bonds well to Al? I believe I had read somewhere that it isn't a
very good one.

Thomas

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing