A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Dehydration bake
Dehydration bake
2009-02-07
Evelyn B
2009-02-08
Edward Sebesta
2009-02-08
[email protected]
2009-02-08
Bill Moffat
2009-02-09
Yinyan Gong
Dehydration bake
Evelyn B
2009-02-07
I have seen dehydration bakes used as part of solvent cleaning of glass and
sapphire substrates. What is the purpose/advantage of this bake?


EVELYN BENABE
Graduate Research Assistant
RF Microsystems Research Group
University of South Florida
4202 East Fowler Avenue
Tampa, FL 33620
Office: ENB 412
Office Phone: (813)-974-4851
Email: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.