A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: CCD in plasma chamber
CCD in plasma chamber
2009-03-06
Hakemi, Ghazal [SAS]
2009-03-06
Andrew Sarangan
2009-03-06
Brent Garber
2009-03-08
Hakemi, Ghazal [SAS]
2009-03-08
Brad Cantos
2009-03-06
Bill Moffat
CCD in plasma chamber
Hakemi, Ghazal [SAS]
2009-03-08
Dear Brent,

Thank you for your reply, I think Your method would suit my purpose.
The only thing I don t understand is the setup: how do you manage to put laser
and detector outside the chamber and get an image? Are these two components just
kept outside the plasma range? Is that what you are trying to do? Why do you use
HeNe laser? Is it because it is not disrupted by the frequency in the chamber?
Also one more question:  what type of photodetector do ypu use? is it a CCD?

Many thanks again.

Regards.

Ghazal

________________________________________
From: Brent Garber [[email protected]]
Sent: Friday, March 06, 2009 8:23 PM
To: General MEMS discussion
Subject: Re: [mems-talk] CCD in plasma chamber

Ghazal,

I bounce a HeNe laser off my sample and it reflects on to a photo
detector which is connected to a strip chart recorder.  The laser and
detector are outside the chamber.

Brent
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing