MEMSnet Home: MEMS-Talk: effects of glass thickness on anodic bonding
effects of glass thickness on anodic bonding
2009-05-03
tarun mudgal
effects of glass thickness on anodic bonding
tarun mudgal
2009-05-03
hii

I am bonding glass wafers of different thicknesses to siliocn wafers and
found the time taken is increasing, moreover the number of air bubbles
also found to be increased.

does anybody have the precise explanation for that behaviour.
moreover i would like to know the effect of increasing oxide thickness on
bonding parameters.

thnx
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing