Bearing holes in pyrex/glass wafers
2009-05-01
김태진
2009-05-01
Mehmet Aykol
2009-05-01
Kirt Williams
2009-05-02
Brian Stahl
2009-05-02
[email protected]
2009-05-02
Xiaoguang Liu
2009-05-02
Jackgong Hotmail
2009-05-02
HENRI FLECHNER
2009-05-03
Jackgong Hotmail
2009-05-04
Fei Wang
2009-05-04
Robert MacDonald
2009-05-06
김태진
2009-05-04
%Mihaela Carp
2009-05-02
HENRI FLECHNER
2009-05-03
tarun mudgal
2009-05-05
Jackgong Hotmail
2009-05-04
Tomblin, Graham
Bearing holes in pyrex/glass wafers
%Mihaela Carp
2009-05-04
You can use sand blasting machine; you can fit different nose and have
different holes dimension.

Best regards,
Mihaela

________________________________

From: Jackgong Hotmail [mailto:[email protected]]
Sent: Sun 03-May-09 1:07 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Bearing holes in pyrex/glass wafers



I also have the same question. But I want to drill a array of holes =
through
glass or any other transparent(to visible light) materials and the =
diameter
is around 400 micron. Hope some one can help us.

Gong

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.