MEMSnet Home: MEMS-Talk: problem with DRIE
problem with DRIE
2009-06-10
saravan kallempudi
2009-06-10
Bob Henderson
2009-06-11
Michael D Martin
2009-06-11
Karolina psychowlosy
problem with DRIE
saravan kallempudi
2009-06-10
Hello all,

We are trying to ash polymer layer using DRIE with O2 plasma.
We observe purple pink color plasma and the process was never successful.
Plasma parameters are 100W, 0.2 mbar.

Please suggest me!!

Thanks,
Saravan