Hi All,

I am trying to model lift-off in Coventorware. In the tutorials they say
metal thickness should be negative and smaller than photoresist thickness to
achive the final metal thickness. I tried to give negative value but the
program doesn't accepted.

Is there anyone has such an experience to model lift-off in Coventorware
process editor ?

Thanks

Yasin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics