A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to clean silicon wafer after a bad lift-off
How to clean silicon wafer after a bad lift-off
2009-07-21
Shah, Forum N
2009-07-22
Phillipe Tabada
2009-08-07
walter
2009-07-22
Michael Cooke
How to clean silicon wafer after a bad lift-off
Michael Cooke
2009-07-22
You could try piranha then HF

Dr Michael Cooke
Electronic Device Process Scientist

PETEC (The Plastic Electronics Technology Centre)
part of the CPI Group (Centre for Process Innovation)

NETPark,
Thomas Wright Way,
Sedgefield,
County Durham TS21 3FG

T:  +44 (0) 1740 625 717 (office)/+44 (0)1642 442 480 (lab)
F: +44 (0)1642 447 298

www.ukpetec.com
www.uk-cpi.com


-----Original Message-----
From: Shah, Forum N [mailto:[email protected]]
Sent: 21 July 2009 22:11
To: [email protected]
Subject: [mems-talk] How to clean silicon wafer after a bad lift-off

Hello All,

Can anyone tell me how to clean the Silicon wafers after doing lift-off
process (bad lift-off)? So that I can re-use the wafer. I know we use HF
for cleaning the wafers but I am not sure of the exact protocol. Any
suggestions would be appreciated.

Thanks
Forum

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation