A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift- off Ti/Pt
Lift- off Ti/Pt
2009-08-20
Shah, Forum N
2009-08-20
Ruiz, Marcos Daniel (SENCOE)
2009-08-21
Huihang Dong
2009-08-21
DongJuan Xi
2009-08-21
Xiaoguang Liu
2009-08-21
Huihang Dong
2009-08-21
Brad Cantos
2009-08-22
Xiaoguang Liu
2009-08-22
Wilson, Thomas
2009-08-22
Brad Cantos
2009-08-21
mikas remeika
2009-08-22
Wilson, Thomas
2009-08-22
Brad Cantos
Lift- off Ti/Pt
Ruiz, Marcos Daniel (SENCOE)
2009-08-20
In my experience both seem to work pretty well.  If you use Ti, do not
expose the device to HF after patterning the metal.

Dan

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Shah, Forum N
Sent: Thursday, August 20, 2009 2:34 PM
To: General MEMS discussion
Subject: [mems-talk] Lift- off Ti/Pt

Hello All,

I am sputtering a 250 Angstrom adhesion layer of  Ti and 1500 angstrom
adhesion layer of Platinum.

Can someone tell me how long does it take for the lift - off to occur if
the PR thickness is around 7 microns.

And also if someone can tell me if Chrome or titanium is a better
adhesion layer for Platinum.

Thanks in Advance,

Forum
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation