Re: Emissivity Tables for Silicon
1998-10-21
[email protected]
1998-10-21
Ram N. Ramanan
1998-10-21
Fahrettin Levent Degertekin
Re: Emissivity Tables for Silicon
Ram N. Ramanan
1998-10-21
The best source that I have found so far is the following
paper
"Temperature dependent emissivity of Silicon related materials
and structures", IEEE trans. on semiconductor manufacturing,
Vol 11, No. 1, Feb. 1998.

If there are other comprehensive ones, I would like to hear
about those too...

Cheers,
Ram
--
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=
  Ram N. Ramanan, Ph.D.               FSI International
  Microlithography,  R&D              MS 5-7060, 600 Millennium Dr.
  Ph: 972-643-2213                    Allen, TX-75013
  Email: [email protected]        www: http://www.fsi-intl.com
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation