A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: reference for what cricible to use for e-beam
reference for what cricible to use for e-beam
2009-10-23
l j
2009-10-23
Ajay Rajgadkar
2009-10-24
Ruiz, Marcos Daniel (SENCOE)
2009-10-24
Andrew Sarangan
2009-10-24
Prasanna Srinivasan
reference for what cricible to use for e-beam
Ruiz, Marcos Daniel (SENCOE)
2009-10-24
K.C.,

It matters because in some cases materials are simply incompatible at high
temperature.  For example, you wouldn't want to evaporate silver out of a copper
crucible because the materials would form an alloy and your silver source would
be contaminated with copper.

This site has a pretty extensive set of tables:

http://www.lesker.com/newweb/menu_depositionmaterials.cfm?section=MDtable&init=s
kip

Dan

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of l j
Sent: Friday, October 23, 2009 1:50 PM
To: [email protected]
Subject: [mems-talk] reference for what cricible to use for e-beam

Hello group,

Could anyone point me to a reference for what kind of crucible should be used to
e-beam a given material. I haven't found much on-line to my surprise.

The deeper question then, is there a reference for why it matters. From
experience I have found some materials behave better in moly versus graphite,
but to doesn't seem to be directly or only related to the melting point of the
material.

Thank you in advance.

K.C.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group