Hi all,

I'm trying to modify the surface of PDMS by using a wet chemistry approach
illustrated by Guodong Sui et al in Anal. Chem., 2006, 78 (15), 5543-5551.

In this approach a PDMS  channel was flowed with an oxidizing acid solution
(H2O/H2O2/HCl, 5:1:1) to form silanol groups for subsequent attachment of
bioactive compounds.

I'tried to perform this process in various condition (time, temperature,
concentration) without any changes in the surface hydrophilicity and chemistry
(contact angle and ATR/FTIR).

Does anyone know a wet procedure to oxidize the PDMS surface or a reference
(papers, books)  where is described the reaction involved in this process??

Thank you all, I'm looking for you kind reply.

Edmondo Battista, Ph.D. Student in Ingegneria Biomedica e Informatica, UMG
[email protected]
Laboratorio Biomateriali,
4° piano Edificio Bioscienze, Campus "S. Venuta" di Germaneto
88100 - CATANZARO (CZ)
09613694307 - 3280663727
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics