1998-10-26
I'd like to perform mechanical modelling on ferroelectric thin film.
Therefore i need Young modulus, Poisson
coefficient and thermal coefficient of : PbTiO3, MgO, BaTiO3 and SrTiO3.
Does anyone know of published work
giving the mechanical properties of thin films of these materials?

Thanks,

L. Lahoche
/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\
Laurent LAHOCHE
Université de Picardie Jules Verne
33, rue Saint-Leu
80039 AMIENS Cedex 01
Tel : (33) 3 22 82 78 84
Fax : (33) 3 22 82 78 91
\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing