MEMSnet Home: MEMS-Talk: Problem for etching PMMA using RIE
Problem for etching PMMA using RIE
2009-12-20
Chih-Chieh Cheng
Problem for etching PMMA using RIE
Chih-Chieh Cheng
2009-12-20
Hi,

Please take look at this picture:
http://picasaweb.google.com.tw/ccjmc1977/Switch#5417217340388044546

As can be clearly seen in the picture, these black spots are
unwanted deposition (4000 A - 5000 A-thick) which were produced during
etching PMMA (1 um -thick) using O2 RIE. The RIE tool we were using is
Oxford 80 Cloey. Does anyone know what these black spots are  and how can I
avoid and remove them?

Thanks

CC
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing