MEMSnet Home: MEMS-Talk: Dilution of Polyimide
Dilution of Polyimide
2010-01-06
James Paul Grant
2010-01-06
Sue Carter
2010-01-06
Bill Moffat
Dilution of Polyimide
Sue Carter
2010-01-06
James,

I make thin Polyimide films. I use Parylin thinner from HD Microsystems. If
you need more information e-mail me at [email protected]

S. Carter

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of James Paul Grant
Sent: Wednesday, January 06, 2010 3:39 AM
To: General MEMS discussion
Subject: [mems-talk] Dilution of Polyimide

Hello all,

Has anyone got an experience of diluting polyimide or more specifically
polyimide from HD Microsystems?

Thanks,

James

--
Dr. James Paul Grant
Postdoctoral Research Associate
Microsystems Technology Group
74 Oakfield Avenue Room 5
University of Glasgow
Glasgow
Scotland
G12 8LS

Telephone: +44(0)141 330 6690

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Nano-Master, Inc.