[email protected]
2010-01-07
Adamson, Steve
Wafer surface protection UV tape for dicing
[email protected]
2010-01-08
The device is on glass?

If it is for protection from the possible mechanical damage,i.e.
fracture, some sticky blue tape very common in the lab can be used. It
can be easily peeled off. But I don't know the vendor's name. Check
Fisher or macmaster.


Maggie

Quoting Bill Moffat :

> Dan,
>     Protection against what.  If just moisture a deposited hydrophobic
> film helps.  Bill Moffat
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing