MEMSnet Home: MEMS-Talk: Multiple layers HSQ or Fox16
Multiple layers HSQ or Fox16
2010-01-25
James Paul Grant
2010-01-26
Andy Irvine
Multiple layers HSQ or Fox16
James Paul Grant
2010-01-25
Hello,

I would like to spin multiple layers of Fox 16 (aka HSQ) e-beam resist.
I have tried a couple of times to do this but I only end up with a
resist thickness after development of around 1.1 times that of a single
coating step.

Does anyone have any ideas?

Thanks,

Dr. James Paul Grant
Postdoctoral Research Associate
Microsystems Technology Group
74 Oakfield Avenue Room 5
University of Glasgow
Glasgow
Scotland
G12 8LS

Telephone: +44(0)141 330 6690

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.