KOH+IPA
2010-01-24
Andrea Mazzolari
2010-01-25
Maria Matschuk
2010-01-26
[email protected]
KOH+IPA
[email protected]
2010-01-26
A great reference is:

Anisotropic Etching of Crystalline Silicon in Alkaline Solutions (part I and II)
H Seidel, L Csepregi, A Heuberger,
J. Electrochem. Soc., Volume 137, Issue 11, pp. 3612-3626 (1990)