XeF2 gas etch plexiglass?
2010-01-26
Jiho Song
2010-01-26
Kyle Lebouitz
2010-01-26
shay kaplan
XeF2 gas etch plexiglass?
shay kaplan
2010-01-26
It does not but the reaction is exothermic - if you etch a lot of silicon
fast the heat might distort the plastic

Shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Jiho Song
Sent: Tuesday, January 26, 2010 2:54 AM
To: General MEMS discussion
Subject: [mems-talk] XeF2 gas etch plexiglass?

Hello all,

Do you guys know Xenon Difluoride etches the plexiglass?

I am planning to bond the molded Si chip with polymer onto the
plexiglass and put it into the chamber.

Please let me know if you any ideas.

Thank you.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing