MEMSnet Home: MEMS-Talk: Carbon nanotube printing?
Carbon nanotube printing?
2010-02-14
Peng Peng
2010-02-16
Roger Shile
2010-02-16
Peng Peng
Carbon nanotube printing?
Roger Shile
2010-02-16
What size features do you want to print and what length nanotube do you
need? Are you interested in single wall or multiwall nanotubes?

Roger Shile

-----Original Message-----
Dear all,

I heard about some techniques to print out carbon nanotube directly on
the
substrate. This seems an interesting process to me and I am wondering if
any
of you have experience on this. Is there company can handle this sort of
printing?

Thanks and happy valentine's day!

Peng Peng
Graduate Research Assistant
Department of Mechanical Engineering
University of Minnesota
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer