A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: P1-2525 remove from Si
P1-2525 remove from Si
2010-06-03
Darren Alvares
2010-06-03
Huihang Dong
2010-06-07
Darren Alvares
2010-06-07
Huihang Dong
2010-06-04
Paul Nguyen
2010-06-06
Bill Moffat
2010-06-10
Darren Alvares
2010-06-12
Bill Moffat
2010-06-15
Darren Alvares
P1-2525 remove from Si
Paul Nguyen
2010-06-04
 Hi Darren,

I'd agree with Huihang on not using any glue layer such as HMDS if you want
to have PI peeled off after develop.  You may increase the develop time to
2x or 3x for the same purpose.
Hope this helps,
Paul

> ---------- Forwarded message ----------
> From: Huihang Dong 
> To: 
> Date: Thu, 3 Jun 2010 15:17:49 +0000
> Subject: Re: [mems-talk] P1-2525 remove from Si
> Hi Darren,
>
> I have used PI-2611 for my project.
>
> Don't use any of adhesion promoter before your spinning if you want to
> peel the PI.
>
> After your fabrication steps, you can try some sharp
> tools to remove it from the wafer carefully.
>
> The trick is your device may peel off when ultrasonic or auto washing
> are used.
>
> And be careful when acetone is used  during the fabrication, because
> even well cured PI will absorb small amount of acetone which may peel
> your device off the wafer. This will happen more when any bubble appears
>  on your wafer after the spinning.
>
> Hopefully it will help a little bit.
>
> Huihang
>
> > From: [email protected]
> > To: [email protected]
> > Date: Thu, 3 Jun 2010 10:09:55 +1000
> > Subject: [mems-talk] P1-2525 remove from Si
> >
> > Hi All,
> >
> > Just have a question about removing polyimide from an Si Wafer and wanted
> to know if anyone had experience with this? I would spin and bake the PI on
> the wafer. After fabricating the device I wanted to peel the PI with the
> device of the wafer (so it is on a flexible substrate)
> >
> > Are there any special tricks or rigs that you use?
> >
> > Any help I am sure would be very useful
> >
> > Thanks,
> >
> > Darren Alvares
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer