MEMSnet Home: MEMS-Talk: Etching indium
Etching indium
2010-06-23
Andrew Irvine
2010-06-23
Brent Garber
2010-06-24
Andrew Irvine
Etching indium
Brent Garber
2010-06-23
Andrew,

Are you still using indium to mount your wafers in your MBE?  I stopped
using that method 10 years ago and found VEECO sells wafer holders and
custom holders for small pieces.
I would think spinning photo resist on your front side and a good bake
would provide plenty of front side protection if you still want to do a
wet etch.  Back when I did 1cm squares, I would use resist on the front
and a cotton swab with nitric acid for a quick clean up of the indium.
I didn't care about back side damage.

Brent

Andrew Irvine wrote:
> Hi all.
>
> Anyone out there have to etch indium from the back surface of their GaAs
> wafers after MBE growth?
>
> Any thoughts on how I can do it?
>
> Boiling conc HCl seems to do half a job (some kind of rough residual
> crud left over), and I can't find a suitable way of protecting the
> epitaxial surface.
>
> Yep, I'm asking the growers too!
>
> Many thanks,
>
> Andy
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.