Darren,

       Lots of questions.  How thick is your resist? What is the process
you are using to try for a reverse slope of your resist edge?  Contact
me directly for lots of papers on lift off techniques.

[email protected]


Bill

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of [email protected]
Sent: Monday, August 16, 2010 5:45 AM
To: [email protected]
Subject: Re: [mems-talk] Lift Off

Hi Darren,

indeed, your lithography looks ...hm... not good. I'll guess, no
lift-off possible.

Something is really wrong with your litho. It could be: mask not in
contact with substrate or wrong focus. Too low dosis (looking at 10um
line). Old or contaminated resist/developer. Wrong processing order? Try
to check this first with other users. 10um lines should be very easy to
pattern.

Furthermore, what is you substrate? Could it be that your (alkaline)
developer attacked the substrate?

Best
Daniel
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics