MEMSnet Home: MEMS-Talk: Dry film photoresist for electroplating
Dry film photoresist for electroplating
2010-09-15
Mingke Xiong
2010-09-15
Bill Moffat
2010-09-16
shay kaplan
Dry film photoresist for electroplating
Bill Moffat
2010-09-15
Possibly DuPont Riston developed for PCB manufacturing.


Bill Moffat, CEO
Yield Engineering Systems, Inc.
203-A Lawrence Drive, Livermore, CA  94551-5152
(925) 373-8353

www.yieldengineering.com


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of Mingke Xiong
Sent: Wednesday, September 15, 2010 2:10 PM
To: General MEMS discussion
Subject: [mems-talk] Dry film photoresist for electroplating

Hi guys,

Does anyone know a good and cheap type of dry film photoresist that has
good adhesion to PCB (Cu surface)? We want to use the PR mold for Zn/Sn
plating. The minimum feature is about 50~60 um width straight lines.

Thank you.

Regards,

Mingke Xiong
AEM, Inc.
6610 Cobra Way
San Diego, CA 92122, USA
www.aem-usa.com
858-481-0210 (1660)
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing