Parasitic capacitance associated with planar inductance on Si
2010-09-28
Christian Engel
2010-09-28
ning xue
2010-09-28
Albert Henning
Parasitic capacitance associated with planar inductance on Si
ning xue
2010-09-28
Hi Chris,

There is magnetic energy loss in your n-type silicon and the silicon oxide
layer is too thin. If you want to decrease the parasitic cap, there are
several ways.

1. use very thick sio2
2. use air bridge as isolating layer
3. use glass substrate instead of silicon.

As I know, the third method is very good. I use this method. The paracitic
cap is only 0.1-0.2pf

Thanks



2010/9/28 Christian Engel 

> Hello people,
>
> At the moment we are trying to build planar inductivities on an n-type
> Si-wafer. Currently, there is an SiO2-insulator of about 50nm thickness
> between substrate and the structured, sputtered Cu-Layer that forms the
> inductivity.
>
> Unfortunately, a parasitic capacitance of some dozen nF can be measured
> while trying to measure the completed inductivities. Can anybody give me an
> idea for being able to explain this problem?
>
> Thanks in advance and best regards, Chris
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review