MEMSnet Home: MEMS-Talk: silver nano paste
silver nano paste
2010-09-29
Mingke Xiong
2010-09-30
Alex Mellnik
2010-10-01
Mingke Xiong
silver nano paste
Mingke Xiong
2010-09-29
Hi all,

I am wondering if anyone has some experience with how to make silver nano paste
out of silver nano powder, or maybe has a reference where I can find such
information.

Our plan is to screen print the silver paste onto PCBs serving as seeding layer
for electroplating. Right now we have some silver nano powders with 40~90nm
dimension. We want to find out what is the best way to disperse the powder into
solvent, a good coating method, proper baking temperature, etc.

Thank you all in advance.

Regards,

Mingke Xiong
AEM, Inc.
6610 Cobra Way
San Diego, CA 92121, USA
858-481-0210 (1660)
www.aem-usa.com
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing