MEMSnet Home: MEMS-Talk: Damaged wafers after SC1 clean
Damaged wafers after SC1 clean
2010-10-21
Fradkin Evgenia - Golda
2010-10-21
Felix Lu
2010-10-21
Goodman, Lawerence
Damaged wafers after SC1 clean
Fradkin Evgenia - Golda
2010-10-21
Hello,

We've encountered a serious damage to the wafers surfaces during SC1 cleaning
process.  A picture of a damaged silicon wafer after the cleaning process is
attached.
This damage occurs only for wafers from a certain vendor.

It seems that wafers from other vendors are damaged as well if being cleaned in
the same solution after the said damaged wafers.

Have anyone encountered such a problem before? Can you suggest what might be the
cause?

Thanks,

Evgenia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.