A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: copper plating
copper plating
2010-10-26
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-28
Fei Wang
2010-10-28
Mingke Xiong
2010-10-27
Kuijpers, Peter
2010-10-27
Mingke Xiong
copper plating
Mingke Xiong
2010-10-28
Hi, Fei,

Thank you for the advise!!! I should have thought of that!! Thank you!

Regards,

Mingke Xiong
AEM, Inc.
6670 Cobra Way
San Diego, CA 92121, USA
858-481-0210 ext. 1660
www.aem-usa.com

________________________________________
From: [email protected] [mems-talk-bounces+mxiong
[email protected]] On Behalf Of Fei Wang [[email protected]]
Sent: Thursday, October 28, 2010 1:36 AM
To: General MEMS discussion
Subject: Re: [mems-talk] copper plating

Hi, Mingke,

You can try to combine your forward current pulse with a reverse cycle.

Best regards,
Fei
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review