MEMSnet Home: MEMS-Talk: Uneven surface thickness of SU-8 2100
Uneven surface thickness of SU-8 2100
2010-12-01
Nirmal punjabi
2010-12-01
Alex Mellnik
2010-12-02
[email protected]
2010-12-02
Xiaohui Lin
2010-12-02
Michael Riss
Uneven surface thickness of SU-8 2100
Alex Mellnik
2010-12-01
In my experience SU-8 2000 series can develop really large edge beads,
especially on small substrates.  I imagine that only spinning at 800 rpm
can't help much either.

-Alex

On Wed, Dec 1, 2010 at 12:30 PM, Nirmal punjabi wrote:

> Hi,
>
> I need a thickness of around 400um of SU-8, i am spin coating SU-8 2100 at
> 800rpm for 60 sec.
>
> But the final structure formed has uneven surface.
>
> Can anyone help me on this matter?
>
> Thank you.
>
> Nirmal.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.