A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: spin coater vacuum path
spin coater vacuum path
2010-12-09
Jia Yao
2010-12-09
Andrew Sarangan
2010-12-09
Jia Yao
2010-12-09
Brad Cantos
2010-12-09
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Morrison, Richard H., Jr.
2010-12-10
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Shay
2010-12-09
Andrew Sarangan
2010-12-10
David Grove
2010-12-09
ZijianCao
2010-12-09
Jia Yao
2010-12-10
Huy
2010-12-13
Jia Yao
2010-12-14
Paul Grasso
spin coater vacuum path
Andrew Sarangan
2010-12-09
Probably the blockage has moved further downstream, and into the
vacuum solenoid. Try removing the solenoid and cleaning it.


On Wed, Dec 8, 2010 at 7:33 PM, Jia Yao  wrote:
> Hi all,
>
> I am having problem with spin coater. At first there were some photoresist
> going into the chuck all the way to the bottom so the program stopped
> automatically after a couple of seconds of running. Also the platform was
> very hard to rotate by hand. After I cleaned the pathway which has the
> photoresist, the platform moves freely but the vaccum is showing
> insufficient value. Is there something blocking the vacuum
> somewhere? How could I possibly check the block?
>
> Thank you very much!
>
> Jia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics