MEMSnet Home: MEMS-Talk: SU-8 3000 vs 2000 adhesion
SU-8 3000 vs 2000 adhesion
2010-12-11
Mikael Evander
2010-12-11
Bill Moffat
2010-12-12
Mikael Evander
2010-12-12
Andrew Sarangan
2010-12-12
Gareth Jenkins
2010-12-13
Bill Moffat
2010-12-13
Bill Moffat
2010-12-13
Yifan Wu
2010-12-15
Adrian Papas
2011-01-28
Mikael Evander
2011-01-28
Andrew Sarangan
2011-01-28
Mikael Evander
2011-01-28
Andrew Sarangan
2011-01-28
Dietrich Lueerssen
SU-8 3000 vs 2000 adhesion
Adrian Papas
2010-12-15
Hey Bill,

What kind of substrates do you implement the APTES adhesion promoter +
SU8 combination, and which SU8 series do you use? I'm just curious
because our process/research does the reverse where we lay down the SU8
first and then perform an APTES treatment on top of everything (we use
the APTES for another purpose, not as an adhesion promoter). It might be
interesting to perform it in the reverse fashion. Thanks.

Adrian Papas

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing