MEMSnet Home: MEMS-Talk: etch rate of Ag in XeF2
etch rate of Ag in XeF2
2011-01-07
Tricia Youngbull
2011-01-08
Robert Ditizio
2011-01-08
Paul Sunal
2011-01-08
[email protected]
2011-01-08
[email protected]
2011-01-08
Ned Flanders
etch rate of Ag in XeF2
[email protected]
2011-01-08
RIE or ICP?


------Original Message------
From: Paul Sunal 
To: General MEMS discussion 
ReplyTo: Paul Sunal 
Re: [mems-talk] etch rate of Ag in XeF2
Jan 7, 2011 20:06

Tricia,

It does!  But in a complex manner.  I don't have the etch rate, but I
know from experience that the Ag undergoes some sort of chemical
reaction and then etches away.  It is slower than the etch rate of
silicon, but still fairly fast.

Regards,

Paul
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing