Antistick layer for nanoimprinting
Shay Kaplan
2011-01-20
You can try treating is with HMDS. It's not the best but you probably have
some around

Shay

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Xiaohui
Lin
Sent: Wednesday, January 19, 2011 6:20 PM
To: General MEMS discussion
Subject: [mems-talk] Antistick layer for nanoimprinting

Hi:

    We are doing nanoimprinting using mold with Ni finish (all pattern are
in Ni). Could anyone suggest an anti-stick layer material that can render
the surface more hydrophobic?

Thanks.

--
Lin, Xiaohui
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing