MEMSnet Home: MEMS-Talk: Protek adhesion problem
Protek adhesion problem
2011-02-07
Temmuz
2011-02-07
Warren Dustin
2011-02-08
Bill Moffat
Protek adhesion problem
Temmuz
2011-02-07
Hi,

I am trying to etch 500um Si wafer with %30 KOH at 80C.  I bought Protek
PSB coating in order to protect my front side however the adhesion is
very bad.  Does anybody have intel about this issue and how to overcome?

Thanks in advance


Temmuz CEYHAN
M.Sc. Student
-----------------------------------------------
Dept. of Electrical and Electronics Engineering
+90(312)-290-1247
Advanced Research Labs / National Nanotechnology Research Center
+90(312)-290-3525
BILKENT UNIVERSITY
06800
ANKARA/TURKEY
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.
Tanner EDA by Mentor Graphics