A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Sloped microchannel
Sloped microchannel
2011-02-28
Tsoll Doiiu
2011-02-28
Nabhiraj Yalagoud
2011-02-28
Dr. Holger Becker
2011-03-04
khan waseem
2011-02-28
Dietrich Lueerssen
2011-02-28
Nabhiraj Yalagoud
2011-02-28
Kevin Nichols
2011-02-28
Bill Moffat
2011-03-01
Kevin Nichols
2011-03-01
Shao Guocheng
2011-03-11
eowin rohan
Sloped microchannel
Tsoll Doiiu
2011-02-28
Hello MEMS community!

Does anybody have an idea how to prepare a sloped microchannel in PDMS?

Initially I've tried to do like this: spin-coat PR on Si wafer, than hold the
wafer vertically,
for like a 1h-4h, hoping  that gravity will make gradient in PR thickness, than
make UV.
Unfortunatelly, I did not achieve the slope. I used SU 25 for this.

Is there some other way to prepare oblique microchannel?
The desired sizes are: length - approx. 4cm, initial heigth 200um, final heigth
20um.

I want to make like this:
http://img193.imageshack.us/img193/5440/46006411.jpg

Also the ways to prepare slopes with angles 30-70 degrees are strongly wanted.

Thanks in advance!


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing