MEMSnet Home: MEMS-Talk: SU-8 bonding?
SU-8 bonding?
2011-04-06
samira movahedian
SU-8 bonding?
samira movahedian
2011-04-06
Dear All,

Could anybody help me with SU-8 bonding? I'm trying to bond two layers of
SU-8 (one 40µm and the other one 10µm) to each other, but I haven't
succeeded yet. Does anybody know  what the best method is? I would
appreciate it in advance.


Cheers,

samira