Bonding gold to Niobium?
2011-06-02
Jie Zou
2011-06-02
Roger Shile
Bonding gold to Niobium?
Jie Zou
2011-06-02
Hi, folks,

I know it is the best to use Al as the bonding wires for Niobium.
Unfortunately we don't have a Al bonder. Anyone have experience with bonding
gold to Niobium?

Or, can I evaporate gold on the Nb at the bonding area and then do the bonding?

Any care I need to take in order to let the gold and Nb adhere and conduct
well?

Thanks.

*  Zou Jie (Jay)
*  Department of Physics
*  University of Florida
*  Email: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review