MEMSnet Home: MEMS-Talk: dicing problem with silicon wafer
dicing problem with silicon wafer
2011-05-31
이요석
2011-05-31
Gary Hillman
2011-05-31
Bill Moffat
2011-05-31
Ruiz, Marcos Daniel (SENCOE)
2011-06-01
이요석
2011-06-02
Jie Zou
2011-06-02
Bill Moffat
2011-06-02
Ruiz, Marcos Daniel (SENCOE)
2011-06-10
Jun Hao
2011-06-10
Ned Flanders
2011-06-10
Bill Moffat
dicing problem with silicon wafer
Jie Zou
2011-06-02
Doesn't HF do that for Si wafers? I don't know for the Pt surfaces.

Jie

On Wed, Jun 1, 2011 at 7:12 AM, �요�  wrote:

> Hello Bill,
>
> How do you do that? Is there a solvent which can make the wafer
> hydrophobic?
> This seems a good idea.
>
> yours,
> Joseph


*  Zou Jie (Jay)
*  Department of Physics
*  University of Florida
*  Email: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics