RIE Etching SiO2/Si
2011-06-06
Judith Linacero Blanco
2011-06-06
Khaled Mohamed Ramadan
2011-06-07
Glenn Silveira
2011-06-06
Andrew Sarangan
2011-06-06
Gary Hillman
2011-06-09
Judith Linacero Blanco
2011-06-09
Judith Linacero Blanco
2011-06-09
Robert Ditizio
2011-06-07
antwi nimo
2011-06-07
SALVADOR_ALCANTARA_INIESTA
RIE Etching SiO2/Si
Judith Linacero Blanco
2011-06-06
Hi all,

Does anybody know how to etch Si with a SiO2 mask? Because I use 50sccm
HBr, 30mT and 200W in the RIE system, but the selectivity isn't good.
I only have 20nm of SiO2 to etch silicon.

Thanks a lot,
Judith
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing