Hello,


I wonder if someone know if old formulations of Shipley photoresists (Microposit
S-1400-37; 1813 and 1828) are available from Rohm and Hass or from Dow. I have
checked the web of Dow and it looked like the resists are discontinued.

Thanks in advance.