MEMSnet Home: MEMS-Talk: Removing oxide from Silver Die
Removing oxide from Silver Die
2011-07-20
Abdul Qader Ahsan Qureshi
2011-07-21
Shay
2011-07-21
Bill Moffat
Removing oxide from Silver Die
Shay
2011-07-21
What's the oxide thickness? Or is it just the black tarnish which is usually
sulfides?

Shay

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Abdul
Qader Ahsan Qureshi
Sent: Wednesday, July 20, 2011 6:32 PM
To: [email protected]
Subject: [mems-talk] Removing oxide from Silver Die

Dear All,

Does anyone know an etching recipe for removing the oxide layer from the
surface of the Silver electroplated die. The thickness of the silver is 200
microns.

Regards
Abdul Qader Ahsan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
MEMS Technology Review