LPCVD silicon nitride on Au grating lines
[email protected]
2011-08-26
I tried to deposit the SiN on top of SiO2/Si layers by LPCVD. There
are some Au structures (40nm thickness with 5nm Ti adhesion layer)
that are deposited by ebeam evaporator on top of SiO2 surface. My aim
is to cover the Au structures evenly. Will this be a problem? Since
our SEM is down, I cannot take SEM pictures now.

Thanks!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review