MEMSnet Home: MEMS-Talk: LOR resist not releasing SU 8
LOR resist not releasing SU 8
2011-10-05
sumit kalsi
2011-10-05
Michael Martin
2011-10-06
Wilson, Thomas
LOR resist not releasing SU 8
Michael Martin
2011-10-05
Hi Sumit,

   What solvent are you using to release the LOR?  My understanding is that
the longer and higher the temperature one uses to bake LOR the harder it is
to solvate.  We have had good luck removing LOR with MF-319 but less so with
acetone.

Cheers,
  Michael

On Wed, Oct 5, 2011 at 8:58 AM, sumit kalsi  wrote:

>
> Dear All,
>
> I am trying to use LOR 5A for release of SU 8 sheets. It worked fine with
> single patterning of SU8. Recently I tried to use it for releasing SU 8
> which is double patterned, but it did not released SU 8. Could it be that
> because of two post bakes that it is not releasing SU 8? I pattern SU 8
> (around 50um) and then after 3-4 hours (because of overnight exposure with a
> laser), post bake it according to specifications given by microchem. Then I
> expose it again and post bake immediately. Develop it after atleast 4 hours.
> Has any one had any experience on this? Any help is much appreciated.
>
> Thanks a lot in advace!
>
> Kind Regards,
> Sumit
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation